⏣ General Metalworking

30775 Threads Posts
to

My "free" ATV

It's a 2007 Arctic Cat 650 and now I know why my neighbor gave it away ... so far I have about 6 or 700 bucks in parts...
2 comments posted 2w
posted by Snag_one
2 comments posted 2w posted by Snag_one

Ali-MIG test-welds pics - diagnose?

Hello all I know previous comments, but - does anyone have any ideas here? http://www.weldsmith.co.uk/greet/cs411/26072...
9 comments posted 3w
posted by null
9 comments posted 3w posted by null

AI Technical Recent Experience

I finally signed up for ChatGPT. I am a little disappointed. Its better than Gemini AI, but it has a lot of same random...
6 comments posted 3w
posted by none
6 comments posted 3w posted by none

Watched tank running day at Bovington (UK) FWIW

For what it's worth... went 2 days ago to Bovington camp tank museum for "running" day - of mainly WW2 armoured vehicle...
15 comments posted 1mo
posted by null
15 comments posted 1mo posted by null

Your Generator Sucks (Maybe Mine Too)

YOUR GENERATOR SUCKS Long read, but maybe worth it Mine does too. If you are on jobs sites using it all the time it pro...
10 comments posted 1mo
posted by none
10 comments posted 1mo posted by none

donut spare and AWD

A large part of why I'm fixing the AWD 2000 CRV is its very conveniently rear hatch mounted full sized spare tire, like...
10 comments posted 1mo
posted by muratlanne
10 comments posted 1mo posted by muratlanne

Should I use hardfacing rod ?

I want to build up the cutting edges on the blades on my brush hog , they're worn and the bottom side is no longer flat...
2 comments posted 1mo
posted by Snag_one
2 comments posted 1mo posted by Snag_one

Re: Homemade diesel hammer???

> >> I was at a construction site with my 4 year old son. It was like a >> heaven for him, both heavy duty construction...
5 comments posted 1mo
posted by Snag_one
5 comments posted 1mo posted by Snag_one

Best Blow Gun

What is the best? Make a model blow gun in your opinion. I keep my shop air regulated at about 125PSI someone that lists...
0 comments posted 1mo
posted by user16941
0 comments posted 1mo posted by user16941

1/4 Turn T-Nuts

Any of you all use these? Instead of having to slide them in from end you can just drop them directly into the t-slot a...
1 comments posted 1mo
posted by none
1 comments posted 1mo posted by none

Refractometer - It Was Worth It

When I first calibrated it and used it the coolant in my machine tanks was basically off scale or at the very top. I ha...
0 comments posted 2mos
posted by none
0 comments posted 2mos posted by none